ANVILFIELD Try FieldOS

Field glossary · measurement

Severity / extent

A severity/extent record pairs a condition rating with a measured quantity and the survey rule used to combine observations. Under FHWA's fifth revised LTPP manual, a 12 m transverse crack with 2 m at high severity is recorded as one high-severity crack totaling 12 m: the damaged segment exceeds the 10% aggregation threshold. The high rating does not mean that every meter has the same opening or that the repair covers a large area.

How bad a distress is (low, medium, high) and how much of the section it covers (area or linear feet)

Used across 2 Anvilfield field guides, most in Paving.
Updated

Which crack widths change the severity rating?

FHWA's May 2014 LTPP manual classifies an unsealed transverse crack with mean width of 6 mm or less as low severity when adjacent random cracking does not raise the classification. The width-only moderate band is greater than 6 mm through 19 mm; a mean width above 19 mm is high. These are mean crack widths, not the largest isolated opening visible in a photograph.

Associated cracking also changes the call. In the LTPP transverse-crack criteria, random cracking within 0.3 m counts as adjacent: low-severity random cracking raises an otherwise narrow crack to moderate, while moderate or high random cracking raises it to high. Measure the opening and inspect the neighboring pavement. A width-only survey misses part of the definition.

When does one bad segment rate the whole crack?

The LTPP manual's 10% length rule makes a useful field calculation. On a 12 m transverse crack, a 2 m high-severity segment occupies 16.7% of the length, so the complete crack receives a high rating. The LTPP record needs both the count, one crack, and its 12 m length under that rating; splitting it into separate severity lengths would change the prescribed measurement.

Longitudinal cracking has different measurement instructions: LTPP records its length at each severity and separates wheelpath from non-wheelpath observations. Keep the distress-specific instructions beside the field form. Applying the transverse-crack rule to every linear distress changes the data even when the tape readings are correct.

Keep rut depth separate from the amount affected

Rut depth describes vertical deformation at a measurement location; it does not say how much pavement is affected. FHWA's LTPP manual preserves measured rut depths or transverse profiles without assigning low, moderate, or high severity levels. Its raveling record uses affected square meters without severity bands, while fatigue cracking uses square meters at each severity.

For fatigue cracking, the same manual assigns an inseparable area of mixed severity the highest severity present. Where boundaries are distinguishable, keep separate measured areas. An 80 sq m fatigue area within a 400 sq m surveyed section occupies 20% of that section; record the severity separately so a later reviewer can distinguish area growth from worsening breakup. That percentage is an area fraction, not a PCI score.

Keep LTPP observations separate from PCI scoring

The active ASTM D6433-24 PCI practice uses its own visual-survey criteria, so an LTPP crack record is not automatically a valid input to its deduct calculation. ASTM's public scope distinguishes surface observations from direct tests of capacity, friction, and ride. A maintenance database should retain a survey-method field rather than combining similarly named distresses from different catalogs.

Use the distress diagnosis guide for mechanisms and the PCI assessment guide for the scoring workflow. Label observations collected under LTPP as LTPP observations; importing them into a PCI worksheet requires resolving the catalog and measurement differences first.

Frequently asked questions

Does high severity mean a large repair area?

Severity and quantity remain separate fields. A short, badly deteriorated crack and a long, narrow crack produce different records. Keep the measured quantity with its classification instead of using the adjective as a repair takeoff.

Can a photo establish crack severity?

A useful image includes a scale and shows surrounding cracking, but the rating also depends on the survey's length, area, and aggregation rules. Tie the image to the crack ID, ruler reading, and measured length used for the aggregation calculation.

Sources checked

Where this shows up

Next step: Build a survey route

Back to the full field glossary