Valve-regulated lead-acid (VRLA) identifies a battery maintained through electrical and temperature measurements; vented lead-acid (VLA) also permits electrolyte sampling and water replenishment. These construction labels do not establish a shared float setting. Compare each cell model's charging sheet at the same temperature, and keep electrolyte-level and density records for vented cells rather than opening a valve-regulated case to take them.

Valve-regulated (sealed) lead-acid and vented (flooded) lead-acid, the two lead-acid families with different maintenance and rooms

Used across 3 Anvilfield field guides, most in Datacenter.
Updated

Float voltage belongs to the cell model and temperature

EnerSys specifies 2.29 V per cell at 20°C and 2.27 V per cell at 25°C for its PowerSafe V Front Terminal and V 2 V DIN-size batteries. A temperature-qualified voltage is a charging condition, not merely a number copied from an old charger label.

For a 240-cell string, those settings calculate to 549.6 V and 544.8 V respectively, a 4.8 V difference across the string. Record the cell temperature basis with the charger target so a later comparison uses the same condition. Include that charger target in the UPS battery test record so the discharge result retains its preceding charge condition.

EnerSys's flooded-stationary instructions specify 2.23 V per cell at 20°C for OPzS and TS tubular cells. This separate product example shows why copying a VRLA float setting into a flooded bank is an engineering change, even when both banks contain lead-acid cells.

What a hydrometer reading means on a vented cell

EnerSys lists a nominal electrolyte density of 1.240 kg/L at 20°C for its OPzS and TS cells at the nominal electrolyte level. Its correction example converts a measured 1.230 kg/L at 35°C to 1.240 kg/L at 20°C. Temperature correction therefore changes how an apparently low reading is interpreted.

EnerSys's flooded-cell instructions place the density reading before water addition or after boost charging, rather than immediately after topping up. Record the electrolyte level and temperature with that reading. The manual calls for annual individual-cell voltage and density readings; every six months it calls for total battery voltage, pilot-cell voltage, density and temperature, and room temperature.

Water replacement is a construction-specific task

EnerSys limits water for its flooded stationary cells to demineralized or distilled water with conductivity no greater than 10 microsiemens per centimetre. The maintenance addition replaces water lost from the electrolyte; routine topping up is not an acid addition.

A VRLA pressure-relief valve is not a watering port. Opening a sealed cell to imitate flooded-cell maintenance defeats the construction being maintained. Keep electrolyte records for vented cells and electrical and temperature trends for valve-regulated cells, with the exact model's instructions attached to each asset record.

Sources checked

Also defined as

  • Sealed valve-regulated and vented flooded lead-acid, recombinant lower-gas versus continuously gassing

Where this shows up

Next step: Follow UPS replacement work