Field glossary · material
Rejuvenator
A rejuvenator changes selected properties of aged asphalt binder, but its dosage basis depends on how it is used. A recycling agent blended into a mix can be dosed against aged binder mass; a surface emulsion is applied over a measured area. In the worked mix calculation, a 5 percent dose against 500 kg of aged binder requires 25 kg of agent. Neither a product classification nor a darker pavement surface establishes the resulting mixture performance.
A product that penetrates and restores aged asphalt binder by replacing lost maltenes, softening it and bringing back flexibility
A recycling-agent classification is not mixture approval
ASTM D4552/D4552M-20(2025) classifies hot-mix recycling agents by kinematic viscosity measured at 60°C, or 140°F. It excludes emulsified recycling agents and does not establish the performance of the resulting binder blend or asphalt mixture. A submittal naming this classification therefore still needs the blend and mixture results required by the job.
Identify the addition point in the recycling production plan, then pair the supplied-agent certificate with the recovered-binder blend results. These describe different materials; keep their sample numbers distinct when assembling the submittal.
What a surface-emulsion data sheet actually measures
Martin Asphalt's Reclamite data sheet lists 60 to 65 percent residue by weight and a residue viscosity of 100 to 200 centistokes at 140°F. Residue content and residue viscosity are different test results: the first describes quantity after water removal, while the second describes the remaining material's flow resistance.
That Martin Asphalt sheet gives a storage range of 50 to 140°F and an application range of 50 to 130°F for its Reclamite product. These are liquid-product temperatures, not a statement that pavement at any temperature within that band is ready for traffic. Put the product's liquid-temperature reading beside the treatment and reopening record for the surface rejuvenation work.
How much agent does a binder-based dosage require?
A 10,000 kg recycled mixture containing 500 kg of aged binder receives 25 kg of agent when the design dose is 5 percent of that aged binder mass. The same 25 kg is only 0.25 percent of mixture mass. Entering 5 percent against the mixture would call for 500 kg, a twentyfold difference.
Put the dose basis on the design, delivery instruction and production record. Surface applications need their own area-based quantity and dilution record instead. For verification of the binder effect, report the specified before-and-after viscosity or rheology results; a darker surface photograph does not quantify how much the binder changed.
Distinctions
- Soft virgin binder
- Changing the virgin binder grade and adding a separate recycling agent are distinct design adjustments. The final blended properties, rather than a product name, establish the resulting binder behavior.
Frequently asked questions
Does a rejuvenator reverse all asphalt aging?
It changes selected binder properties. Demonstrate the required effect with the specified blend and mixture tests rather than treating a dosage or a darker color as proof of restored performance.
Sources checked
Also defined as
- A recycling agent that softens aged RAP binder back toward fresh behavior