Field glossary · property
Scale
A water-side deposit qualifies as scale when dissolved salts crystallize onto the equipment, a distinction Veolia makes from solids carried in as sludge. Measure thickness and identify chemistry before assigning a fuel penalty: DOE estimates 2 percent fuel loss for 1/32 inch of normal scale in a firetube boiler without stack-gas heat recovery, versus 7 percent for iron-plus-silica scale at that thickness. A water-hardness result alone cannot identify that deposit.
A hard mineral deposit, mostly calcium and magnesium hardness, that bakes onto hot surfaces and insulates them
Put a fuel penalty on measured boiler scale
DOE Steam Tip Sheet 7 assigns a 2 percent fuel loss to 1/32 inch of normal-composition scale in a firetube boiler without stack-gas heat recovery. The same sheet assigns 3.1 percent to a high-iron deposit and 7 percent to iron-plus-silica scale at that thickness. Deposit chemistry changes the estimate even when a thickness measurement stays the same.
At 100,000 MMBtu of annual fuel use, applying DOE's 2 percent normal-scale factor identifies 2,000 MMBtu per year associated with the deposit penalty. The measured 1/32 inch thickness is about 0.79 mm. Record boiler type, recovery equipment, composition, and thickness with the estimate; the same thickness on an ice-machine evaporator does not carry this firetube-boiler fuel factor.
Separate surface-grown crystals from deposited sludge
Veolia's Water Handbook distinguishes scale crystallized directly on tube metal from sludge formed elsewhere and carried onto the surface. It also explains that sludge can bake into a hard, adherent deposit. A hard sample therefore does not, by itself, establish where or how the material formed.
Preserve samples from separately identified locations before cleaning mixes the deposits. At a shutdown inspection, record which side of the heat-transfer surface carried each sample, its thickness, coverage, and adhesion. Veolia's handbook identifies crystalline scale constituents by X-ray diffraction; a photograph cannot supply that chemical identification. Carry the laboratory result into the cleaning specification and the boiler-water treatment program.
Why low feedwater hardness does not finish treatment
Veolia reports boiler feedwater hardness commonly between 0.01 and 2.0 ppm and states that internal treatment remains necessary even within that range. Its handbook identifies pressure, heat-transfer rate, boiler design, and steam use as drivers of required feedwater quality.
The CaCO3 unit on a hardness report is an equivalence basis, not a finding that the deposit consists of calcium carbonate. USGS identifies calcium and magnesium as the main contributors to hardness, while Veolia lists several different crystalline scale compounds. Keep the water test and deposit analysis separate when selecting water treatment or diagnosing an ice machine's water-side problem.
Trend stack temperature without changing the comparison
DOE recommends comparing stack-gas temperatures at constant firing rate and excess oxygen concentration when looking for deposit buildup. A temperature rise across unlike firing conditions does not isolate a scale penalty. Save those operating conditions with the temperature trend, then compare the post-cleaning result on the same basis and retain the shutdown inspection findings.
Distinctions
- Copper-oxide scale
- Oxide formed during brazing has a different origin from mineral crystallization out of water. Its prevention belongs to the refrigerant-piping process, rather than a hardness-control program.
Frequently asked questions
Does a zero-hardness sample prove that old scale is gone?
The water sample characterizes water at the sampling point and time. Existing deposits require their own inspection or performance evidence. A successful upstream treatment change and removal of an older deposit are separate findings.
Sources checked
Also defined as
- Plumbing: Calcium and magnesium deposited as a hard crust where water is heated or evaporates
- Hard mineral deposit from calcium and magnesium in hard water, the number one cause of ice-machine failure