ANVILFIELD Try FieldOS

American Concrete Institute

ACI 546: repair compatibility, load sharing, and the construction specification

ACI PRC-546-23 helps the repair designer choose a treatment that restores the intended behavior of existing concrete. A sound repair accounts for the member's load history, material movement, and exposure as well as the damaged volume. ACI 562 supplies the assessment and design code framework; ACI 563 supplies the construction specification. The repair guide connects those decisions without setting one acceptance strength or one patching material for every member.

Current edition: ACI PRC-546-23 (2023)
Updated

Official publisher page

Applies to

Repair designers, restoration contractors, suppliers, and testing agencies need a common description of what each repair restores. Locate the work on the spall restoration plan and identify whether the new material replaces cover, contributes to the load-bearing section, or protects the existing member.

Owners and estimators also need the condition-survey date and the quantity measurement rules. A repair priced by surface area needs a depth category; a volume allowance needs a way to measure irregular removal limits before the patch conceals them.

Key topics

A new patch does not automatically pick up existing dead load

ACI PRC-546-23 explains that repairing a loaded member without relieving its dead load can produce a different final load distribution from the original design. Unloading and reloading sequence therefore affects how the new and existing material share force. The repair drawing should state the intended sequence and load-transfer assumptions, alongside the temporary support design. ACI's public repair-guide preview discusses this under repair design considerations.

Compressive strength alone does not establish compatibility

ACI 546-23 identifies stiffness mismatch, differential creep, shrinkage, thermal movement, and vibration as compatibility concerns between repair material and existing concrete. Equal compressive-strength labels do not demonstrate equal stiffness or volume stability. Ask the supplier for the properties relevant to the design, at the specified ages and service conditions. A high-strength repair that moves differently from its substrate still creates stresses at the interface.

Adjacent demolition can damage a fresh repair bond

ACI PRC-546-23 identifies vibration before adequate repair strength develops as a threat to the interface bond. On a phased garage repair, coordinate nearby demolition and vehicle traffic with the placement and release sequence. Put the affected bays and the release condition on the daily work plan. Protecting the patch face from damage does not control vibration transmitted through the surrounding member.

Use the repair specification to define construction acceptance

ACI SPEC-563-25 supplies construction requirements and specifier checklists for structural concrete repair. The 2025 edition adds coverage including chemical-grout waterproofing, protective membranes, and galvanic-anode cathodic protection. Identify the applicable work sections and complete the project's selections rather than treating ACI 546's overview as an acceptance specification. ACI's 563-25 publication description also distinguishes repair sequencing, material requirements, and acceptance of the work.

Update quantities when deterioration advances after the survey

ACI 546-23 recommends revisiting the condition survey when a considerable delay before repairs allows further deterioration. Use that recommendation to define a preconstruction resurvey and quantity reconciliation. The initial survey date, bid quantities, newly exposed conditions, and accepted repair limits should remain identifiable. This gives an owner a sound basis for changed quantities without confusing added deterioration with a different repair method.

How it is used in the field

Require the repair submission to connect material properties to the repair function. For cover restoration, durability and bond dominate different questions from those governing a section expected to share structural force. Route the product's shrinkage, stiffness, exposure suitability, and application limitations to the designer with the location-specific detail.

At a garage beam, keep the temporary support arrangement and the permanent repair sequence on the same release record. Record when load was relieved, what concrete was removed, when the repair reached its specified release condition, and when support was removed. The parking restoration guide addresses the wider phasing problem; the load-sharing assumption must survive each phase.

An 8-by-12-foot repair at an average depth of 3 inches contains 24 cubic feet, or 0.89 cubic yard. If removal exposes a 4-inch average depth, the volume becomes 32 cubic feet, or 1.19 cubic yards: one-third more material across the same measured face. Record the revised depth and repair limits before placement so the quantity change can be distinguished from a change in repair method.

Retain material batches, placement conditions, test locations, and the accepted disposition with each repair area. Separate strength evidence from interface-bond evidence and from waterproofing results. Each closes a different requirement, especially where one repair combines structural rebuilding and a protective membrane.

Edition history

PRC-546-23 is the 2023 repair guide listed by ACI Committee 546. Its materials-selection companion is PRC-546.3-23, which ACI's catalog records as published in 2024. The suffix is the document designation; the catalog publication year explains that apparent date difference.

Adoption

ACI CODE-562-25 is designed for use with the International Existing Building Code or adoption as a stand-alone repair code. ACI SPEC-563-25 applies through the project specifications. ACI 546 remains guidance for selecting and coordinating methods; the adopted repair code and completed construction documents establish the project's obligations.

Past public repair awards reveal the scale of an agency's restoration program; PorchRocket Bid Control includes previous winners and award amounts alongside upcoming work.

Frequently asked questions

Which document belongs in a concrete repair construction specification?

ACI 563 supplies the reference specification and its project checklists. ACI 546 helps select methods and materials, while ACI 562 establishes the assessment and structural repair design framework.

Will stronger mortar restore a loaded member's original behavior?

The answer depends on compatibility and load history. ACI 546 explains that the existing member's dead load and the unloading sequence affect force distribution, while differences in stiffness and time-dependent movement affect the repaired composite section.

Sources checked

Sections and parts cited

ACI 546R-14

Field guides that apply ACI 546

Browse all codes and standards