ASTM F1869: Calcium chloride calculations and report auditing

ASTM F1869-23 measures concrete-surface moisture output with an anhydrous calcium chloride kit. A reported MVER of 4.3 means an equivalent 4.3 lb of water from 1,000 square feet in 24 hours, rather than 4.3 percent moisture inside the slab. Weighing, net exposed area, and actual exposure time determine the result. The flooring or adhesive manufacturer's specified limit supplies the acceptance decision; F1869 supplies the measurement.

Current edition: ASTM F1869-23 (2023)
Updated

Official publisher page

Applies to

Flooring test agencies, installers, and owners use F1869 when the specified floor system calls for MVER results. ASTM limits the method to applicable bare concrete surfaces and excludes lightweight concrete, gypsum concrete, and tests over coatings, reactive penetrants, patches, or leveling compounds. Product acceptance belongs to the specified flooring system; the test designation supplies a measurement method rather than a universal installation limit. ASTM scope

Key topics

What actually belongs on the scale?

Vaprecision's kit instructions specify a scale graduated in 0.1 gram and direct the technician to reweigh on the same scale. The observation is the sealed dish assembly, including its lid and original sealing tape, at both weighings. A 36.2-gram starting weight and a 38.6-gram finishing weight produce a 2.4-gram gain only if the same components are present. Keep both raw weights with the kit identifier; a final MVER alone conceals a swapped lid or a decimal entered in the wrong column. Vaprecision kit instructions, revised March 2006

Net exposed area explains the conversion factor

Vaprecision calculates its exposed concrete area as 70 square inches inside the cover minus 5.94 square inches occupied by the dish, leaving 64.06 square inches. With that kit geometry, its worksheet uses MVER = mass gain in grams × 118.932 ÷ exposure hours. The coefficient includes the area and unit conversions; it is not a universal constant for every cover. Record the kit model beside the calculation so a replacement kit does not silently inherit another manufacturer's geometry. Vaprecision calculation explanation

A 66-hour result is normalized to 24 hours

Vaprecision's worksheet permits 60 to 72 hours of exposure and rounds the normalized result to the nearest tenth. With its kit factor, a 2.4-gram gain over 66 hours yields 2.4 × 118.932 ÷ 66 = 4.32, reported as 4.3 lb/1,000 ft²/24 h. Using 72 hours for that same observation gives 3.96, understating the rate by 8.3 percent. The collection period and reporting interval serve different purposes: retain the actual timestamps instead of assuming that every kit ran to the maximum duration. Vaprecision exposure and calculation worksheet

How it is used in the field

Price surface preparation, kit deployment, and collection as separate work. Connect the location plan to a worksheet retaining cover geometry, both weights, actual timestamps, and room conditions. Confirm access for the collection visit before setting the first kit; a correct exposure window on paper does not retrieve a kit left behind a locked tenant door.

Treat a broken cover seal, spilled desiccant, or missing weighing component as a compromised measurement. Put that disposition on the location plan and arrange a replacement test. Correcting a spreadsheet does not repair a sample that exchanged moisture with room air through a failed seal.

Audit the calculation before comparing it with the submitted adhesive or coating limit. Preserve the unrounded result in the calculation file and the manufacturer-required reporting precision on the report. When results are close to the acceptance limit, an incorrect time or area assumption can change the release decision without any change in the slab.

A testing firm bidding repeated school flooring packages can reuse its company details through PorchRocket Bid Control, which fills public bid forms from the firm's own file.

Frequently asked questions

Can I reuse the conversion factor from another test kit?

Only when the net exposed area and the manufacturer's calculation are the same. Cover area and dish footprint are part of the measurement geometry. Using a convenient coefficient without identifying its kit leaves the reported rate unsupported.

Why retain both the mass gain and the final MVER?

Mass gain is the observation; MVER is the calculated result. Keeping both allows a reviewer to distinguish a physical test problem from an arithmetic or transcription mistake, and to correct the latter without inventing a new measurement.

Can MVER be converted to in-slab relative humidity?

A kit's mass gain and exposure time cannot produce an F2170 RH percentage. MVER records a surface emission rate; the RH probe samples the slab at depth. When a submitted system asks for RH, add the specified RH testing instead of substituting an MVER result or a conversion chart.