An air barrier is the enclosure's control for air leakage under a pressure difference. Compare material and assembly results separately: CMHA's air-barrier guidance identifies benchmarks of 0.004 and 0.04 cfm/ft², respectively, at 75 Pa. Neither number is a whole-building air-change rate. Field acceptance also needs the installed film thickness and the condition of the connections represented by the test.

A layer or system that stops air leakage through the envelope, rated by air permeance and required to be continuous and sealed

Used across 2 Anvilfield field guides, most in Roofing.
Updated

What an air-barrier test report actually measures

ASTM E2178-21a measures material air permeance and reports it at a reference pressure difference of 75 Pa. Its nominal specimen is 1 m by 1 m. That result describes passage through the specimen; it does not include the roof-to-wall transition, window perimeter, or other connections that make an installed air-control layer continuous.

ASTM E2357-25 measures air leakage through air-barrier assemblies before and after conditioning. The assembly test addresses a different question from the material test: whether the detailed system retains its leakage performance after the prescribed loading. Preserve the assembly drawing with the report so the tested substrate, seams, and penetrations remain identifiable.

Keep the material and assembly limits in separate columns

CMHA's concrete-masonry air-leakage guidance distinguishes a material benchmark of 0.004 cfm/ft² from an assembly benchmark of 0.04 cfm/ft², both at 75 Pa. These numbers are acceptance criteria described in that guidance; ASTM E2178 and E2357 are the test methods used to obtain the corresponding results.

A submitted assembly result of 0.03 cfm/ft² is below the 0.04 assembly benchmark. Comparing it with the 0.004 material benchmark would reject it against the wrong specimen category. Enter the specimen type, test edition, reference pressure, reported result, and applicable project limit on the same review line.

Wet-film thickness belongs on the inspection record

W. R. Meadows specifies 55 mils wet film to produce approximately 23 mils dry film for its AIR-SHIELD LMP application. Those are two stages of the same coating, not interchangeable inspection limits. A wet-film reading is taken during application; a dry thickness describes the film after water has left it.

An inspector recording only "23 mils applied" has left the acceptance question unresolved. Record whether the measurement was wet or dry, the instrument, the substrate, and the location. Consumption over a rough block wall is also affected by surface texture. A bucket count establishes material used; it does not show that thin spots and transitions received the specified film.

Compare pressure and area before comparing results

Keep the leakage units beside the pressure. A material result per square foot and a whole-building result in air changes per hour have different denominators. Changing units alone cannot turn one into the other; building volume, enclosure area, and the relevant test configuration would also be needed.

Use the roof air-barrier guide for continuity through the roof assembly. At submittal review, separate the material sheet, assembly report, and field acceptance record. This prevents a compliant coating certificate from closing an unresolved transition detail.

Distinctions

Vapor permeance
Vapor permeance describes diffusion under a vapor-pressure difference. Air leakage describes bulk airflow under an air-pressure difference; a vapor-permeable coating can still serve as an air barrier.
Air-sealing repair
A repaired opening is a local intervention. Acceptance of the enclosure still depends on the specified assembly details and field test boundary.

Frequently asked questions

Does ASTM E2178 prove that the building is airtight?

No. E2178-21a characterizes material specimens. Installed connections require assembly or field evidence appropriate to the project.

Is wet-film thickness the same as dry-film thickness?

For AIR-SHIELD LMP, W. R. Meadows specifies a 55-mil wet application to obtain about 23 mils dry. A field log must identify which thickness was measured; the two readings describe different stages of the coating.