Field glossary · measurement
Slump
Slump is a vertical drop, reported in inches or millimeters. With a 12 in. mold, a displaced top-center reading 8 in. above the base gives 4 in. of slump. Before treating that number as a delivery result, establish which concrete fraction was sampled and whether the check was preliminary or for acceptance. Those details can explain different readings from one truck without attributing the difference to a changed mixture.
The drop in height of fresh concrete after the cone is lifted, a measure of consistency and workability
Check the cone before changing the concrete
North Dakota DOT's Slump Cone Verification Procedure 38 allows ±1/8 in. on the mold's critical internal dimensions. Its method measures the top and bottom diameters in two directions, turning 90 degrees between readings, and checks the mold height. Measuring only one diameter can miss an oval opening after the cone has been crushed in transport.
NDDOT's calibration record calls for checking acceptance-testing cones before use on a project and independent-assurance cones every 12 months. Those are the agency's equipment-control intervals. Assign the cone an identifier so its inspection record follows the mold that produced the reading, rather than a generic kit number.
Large aggregate changes which concrete gets tested
ASTM C143/C143M-26b, the current slump method, applies directly to plastic concrete with coarse aggregate up to 1-1/2 in. [37.5 mm]. With larger aggregate, the method tests the fraction passing that sieve after the large-aggregate sampling procedure removes the oversize material. Record that preparation so another tester knows which fraction produced the slump.
A sample containing the excluded large particles does not become a valid test simply because the technician can fill the cone. Conversely, a correctly prepared screened sample should not be compared without explanation to an unscreened grab from the same batch. Sample preparation belongs beside the result, especially on mass concrete work.
Preliminary slump is a load-adjustment check
NRMCA CIP 41 describes a preliminary sample obtained after 0.25 yd3 of concrete has been discharged for checking slump and air content before permitted adjustments. The publication advises against making strength specimens from that preliminary sample. Keep this early check identifiable so it cannot be mistaken for the representative acceptance sample used later.
Add sample purpose to the slump test record: preliminary adjustment, acceptance, or check test. Match it to the truck number in the ready-mix delivery record. Retaining the earlier result beside a later result explains the sequence; replacing it with the final number erases which condition was actually tested.
Distinctions
- Equipment tolerance
- A dimensional limit qualifies the mold. It is separate from the specified tolerance used to accept the concrete's slump.
- Slump flow
- Slump flow reports an unconfined spread diameter for self-consolidating concrete. An equipment or sampling error in an ordinary slump test is not a reason to reclassify the mixture as SCC.
Field example
A cone with an 8 in. nominal base measures 8-3/16 in. in one direction and 7-15/16 in. perpendicular to it. Under NDDOT Procedure 38, the first dimension exceeds the 8-1/8 in. upper limit by 1/16 in.; the second is within tolerance. The satisfactory second measurement does not clear the mold. Replace or correct the defective equipment and obtain the required valid test before using the result to justify a mix adjustment.
Frequently asked questions
Does an invalid slump test mean the truck must be rejected?
An invalid test has not established the delivered slump. Correct the identified test defect and follow the specified sampling and check-test requirements so the disposition rests on a valid result.
Sources checked
Also defined as
- A measure of fresh concrete consistency and workability, in inches or millimeters