Field glossary · property
Spalling
Spalling is the breaking away of pieces from concrete or masonry, leaving a cavity or damaged edge. It describes the visible loss, not a single cause. The useful repair description identifies the material, location, depth, exposed reinforcement or connections, and the mechanism still acting on the surface. Those details determine whether a local patch addresses the actual damage.
Cracking and flaking of unit faces, the classic damage from trapping moisture and stress with too-hard mortar
A pavement spall needs a depth decision
FHWA's partial-depth pavement repair guidance limits that repair approach to deterioration within roughly the upper third of the slab. It directs a change to full-depth repair when sound concrete cannot be reached within that depth or when dowel bars are exposed. This is a pavement repair criterion, not a depth allowance for a beam, column, or facade.
FHWA recommends extending pavement repair boundaries 3 to 4 inches beyond the marked delamination or visible spall. The visible cavity therefore does not define the complete removal quantity. Sound the surrounding material and retain the marked limits so the quantity can be reconciled after breakout.
On a 9-inch pavement slab, the upper-third boundary is 3 inches deep. A spall that initially appears shallow but exposes unsound concrete to 4 inches has crossed that partial-depth limit. Widening a surface patch without changing its depth classification would leave the governing defect unresolved.
Brick-face loss and concrete-cover loss need different evidence
National Park Service Preservation Brief 2 warns that mortar hardness is not a reliable proxy for vapor permeability; an old hard lime mortar can remain highly permeable. Its replacement-mortar criteria require separate comparisons of strength and permeability with the units and historic mortar. A compressive-strength result alone cannot establish whether a joint restricts drying enough to explain face loss.
Compare the depth of brick-face loss beside repaired joints with loss beside original joints under the same exposure. Trace water entry above both areas and photograph the unit-to-joint pattern. That comparison tests whether the mortar repair changed performance; a concrete cavity following a reinforcing grid calls for a different investigation of cover and steel condition.
For overhead surfaces, distinguish the material already missing from adjacent detached material still in place. Map both in the condition record. A patch quantity based only on the fallen pieces understates the area that the repair team will encounter.
Write the repair description so it can be measured
Identify each defect by face and location, footprint, maximum and representative depth, fracture condition, and exposed steel. Record cracks or hollow response extending beyond the cavity. Keep the initial survey and final removal dimensions together rather than overwriting the first record.
Put the material and mechanism in the repair description: compatible repointing for the joint condition, concrete defect diagnosis for cover loss. One combined square-foot total cannot convey the different removal depths, materials, and access those scopes require.
Distinctions
- Delamination
- A separated layer can remain in place before breaking away. Spalling records the material loss after a piece detaches.
- Popout
- A popout is a localized loss associated with a particle beneath the surface. It should not automatically be grouped with widespread corrosion-driven spalling.
Frequently asked questions
Does every spall require replacing the whole slab?
The FHWA pavement criterion distinguishes shallow deterioration from damage requiring full-depth repair. Measure the depth and identify the mechanism before assigning the repair extent.
Will harder mortar stop a brick face from spalling?
Measure strength and vapor permeability separately. NPS warns that hardness does not establish permeability, so choosing a higher-strength mortar does not demonstrate better drying or compatibility with the masonry units.
Sources checked
Also defined as
- A deeper surface break than scaling, often at reinforcement or from impact, not a finishing defect