ANVILFIELD Try FieldOS

Field glossary · property

Curling

Curling is curvature through a concrete slab caused by unequal dimensional change between its upper and lower regions. Measure the edge relative to the panel interior and distinguish that shape from a step between adjoining panels. A curled slab can change profile during the day, and an elevated edge does not by itself measure the size of any void beneath it.

Edges and corners of a slab lifting off the base from a moisture or temperature gradient top to bottom

Used across 2 Anvilfield field guides, most in Concrete.
Updated

Measure curvature and faulting as separate results

FHWA's 2012 pavement study defines an upward-curled slab by joints lying above the slab center and a downward-curled slab by the center lying above the joints. A level survey across the whole panel establishes that profile. A straightedge laid only across one joint combines two panel shapes and any permanent step at their interface.

Use a fixed reference outside the area being compared, mark repeatable observation points, and retain the sign of each elevation difference. Record the measurement time and surface condition. Photographing a ruler under a straightedge is useful, but the straightedge span and support points must accompany the photograph.

Reported measurementReference pointsWhat it establishes
Panel edge riseEdge minus center on the same panelCurvature over the recorded span
Joint stepAdjoining edges across the jointDifference encountered by a crossing wheel
Loaded edge movementSame point before and during a recorded loadDeflection under that load, separately from unloaded profile

Why morning and afternoon surveys can disagree

FHWA associates nighttime or early-morning upward thermal curl with the slab top being cooler than its bottom. Daytime surface heating can reduce that upward curve or produce downward curvature. The air temperature alone does not measure the full temperature difference through the concrete.

FHWA-HRT-12-035 reports 10 to 25 inches per mile of IRI reduction at six of eleven Michigan sections surveyed as air temperature rose from 51°F to 74°F over about ten hours. Two sections became rougher and three showed no change. IRI is a road-profile roughness index, so these results demonstrate time sensitivity rather than a floor-edge lift tolerance.

Match the correction to the measured problem

NRMCA CIP 19 distinguishes grinding to restore surface serviceability from under-slab grouting to restore support beneath raised edges. A lower surface profile after grinding does not demonstrate that a support void has been filled. Likewise, a supported edge can still require a separate surface correction.

Repeated panel profiles, joint-step measurements and movement under the intended wheel load separate the shape problem from the support problem. Keep those observations alongside the mix and construction history. Repeat the same measurements after repair so a smoother joint crossing is not mistaken for restored support.

Distinctions

Faulting
A vertical step across a joint. It can accompany curvature but is measured between the adjoining slab faces.
Settlement
Movement of the supporting system or slab elevation. Curling changes slab shape and need not mean the entire panel has settled.

Field example

At 07:00, an edge is 3/16 inch above the same panel's center; at 15:00 it is 1/16 inch above. The measured curvature changed by 1/8 inch. If the step between adjacent panels stayed at 1/16 inch, the survey contains a changing panel shape and a persistent joint step, not one interchangeable 'curl' number.

Frequently asked questions

Does an early flatness test establish the later joint profile?

It records the floor at that test time. Compare later profiles with their temperature, moisture and loading conditions recorded, and measure joint transitions directly when they are the service complaint.

Is a 3/16 inch curled edge a 3/16 inch support void?

Edge rise compares two surface elevations. Void depth requires a reference to the supporting surface beneath the slab, which the top-surface profile does not measure. Record support evidence separately from the rise.

Sources checked

Also defined as

  • Upward warping of slab edges from the top drying and shrinking faster than the bottom

Where this shows up

Related guides

Next step: Build a dock property list

Back to the full field glossary