ANVILFIELD Try FieldOS

Field glossary · method

Exothermic weld

An exothermic weld joins conductors or grounding hardware with molten metal produced by a chemical reaction in a specified mold. Acceptance depends on the finished connection's fill, exposed strands, surface deposits, and porosity. A large weld cap alone is not evidence of a sound joint. Match the mold and charge to the connection, then inspect the cooled weld before it becomes inaccessible.

A metal connection formed by an exothermic process using the specified materials and connection kit

Used across 3 Anvilfield field guides, most in Electrical.
Updated

What makes a cooled grounding weld acceptable?

nVent ERICO's Cadweld inspection guide rejects a connection when slag covers more than 20 percent of its surface or conductor strands remain exposed after slag removal. Those are inspection criteria for the finished connection, not a prediction based on how vigorously the charge burned.

The same guide requires the lowest depression beneath a horizontal connection's riser to remain at or above the top of the conductor. A low fill can indicate too little weld material, metal leakage, conductor movement, or incorrect position. Capture the cleaned connection from an angle that shows the conductor entry and the fill level, not only the top of the riser.

How deep is too deep for a pinhole?

nVent permits a few small pinholes at the riser surface but rejects a pinhole extending beyond the conductor centerline. nVent's inspection method uses a 1/32 in diameter wire to probe depth. Use that dimensional check after cooling and cleaning rather than calling every visible pore a failure or accepting every tall riser.

A 1/32 in probe is approximately 0.8 mm in diameter. The probe size describes the inspection tool; it is not a permitted pore-depth limit. The limiting depth is the conductor centerline. That distinction matters when a small surface opening leads to a deeper internal void.

What the defects tell the next crew

The Cadweld field information guide identifies moisture in the conductor or mold as a cause of porous connections and identifies oil, insulation, and other contamination as additional causes. A repeated defect points to preparation or equipment condition, not a reason to use a larger charge without changing the setup.

A high riser can come from excess charge or contamination, so inspect its surface and fill together. Record the mold identification, conductor sizes and materials, weld material designation, location, and acceptance photo. For ground-ring connections, keep that identification tied to the buried location. For concrete-encased work, capture it before the concrete hides the joint.

Distinctions

Mechanical grounding connector
A mechanical connector is accepted through its listing, application, assembly, and tightening requirements. Weld appearance criteria do not apply to it.
GEC splice
A welded connection to an electrode and a splice joining two lengths of GEC have different code applications, even when the same joining process is used.

Frequently asked questions

Is a silvery weld surface automatically a rejection?

No. nVent describes silvery tin sweat and silver coloration when alloying with certain surfaces. Judge the connection using the guide's fill, strand exposure, slag, and porosity criteria.

Can I accept a weld from a photograph alone?

A clear photograph records visible condition, but a deep pinhole requires the depth check. Complete that inspection while the connection is accessible.

Sources checked

Also defined as

  • A permanent grounding connection fused by a molten-metal reaction, the Cadweld-type

Where this shows up

Next step: Locate outdoor power assets