Exposure class
An exposure class is a design assignment attached to a concrete member, so a mix submittal needs the governing code edition beside the class string. Under ACI CODE-318-25, W1 denotes water contact without a low-permeability requirement, while W2 adds that requirement. F3 from ACI 318-19 has been removed. Those edition differences change how an estimator compares an older exposure schedule with a proposed mixture.
The code category for freezing and deicer exposure that sets the minimum air and maximum water-cement ratio
What belongs beside the class on a mix schedule?
Build the schedule by member location. Record wetting and freezing conditions for F, soil or water sulfate evidence for S, the water-retention requirement for W, and moisture plus external chloride sources for C. Include each assigned class, the code edition and the approved mixture identifier. A producer's mix number or strength label alone leaves those design assumptions unresolved.
Keep soil sulfate percentages and water sulfate concentrations in their original units on the supporting report. A percentage by mass of soil and a concentration in water answer different exposure questions. Link each test location to the member it supports rather than applying a site-average result across unrelated foundations.
What happened to exposure class F3?
NRMCA's March 2026 specification guide confirms that ACI CODE-318-25 removed the F3 exposure class used in ACI CODE-318-19. Freezing exposure and external chloride exposure must still be addressed through their applicable categories; deleting the label does not delete either deterioration mechanism.
An older drawing marked F3 and a new submittal marked F2 are not directly comparable without the full exposure schedule and edition. Read the chloride assignment alongside the freezing assignment. The mix-design guide supplies the proportioning context, while the air-entrainment guide explains the field air measurement.
Water and chloride requirements need separate checks
NRMCA's March 2026 guide summarizes ACI 318-25 W2 requirements as a maximum w/cm of 0.50 for normalweight concrete and a minimum specified compressive strength of 4,000 psi. The code's maximum w/cm limits do not apply to lightweight concrete. W1 and W2 both involve water contact; W2 identifies the additional low-permeability requirement.
ACI 318-25's C2 water-soluble chloride ceiling is 0.15 percent of cementitious mass for nonprestressed concrete, versus 0.06 percent for prestressed concrete, as documented in NRMCA's guide. These are ingredient-chloride limits for the concrete mixture, separate from the external chloride exposure that prompts the C2 assignment.
For a normalweight reinforced slab assigned both F2 and C2, NRMCA's ACI 318-25 summary yields a governing w/cm ceiling of 0.40 and strength floor of 5,000 psi from C2. The F2 air requirement remains applicable. Resolving the ratio and strength does not dispose of the freezing classification.
A chloride submittal with an auditable denominator
Take a proposed nonprestressed C2 mix containing 600 lb/yd³ of cementitious material. Applying the 0.15 percent limit gives 600 × 0.0015 = 0.90 lb/yd³ of chloride ion. A water-soluble chloride result of 0.60 lb/yd³ calculates to 0.10 percent. Write both the analytical basis and the mass denominator beside the result; a percentage of concrete mass cannot be compared directly with a percentage of cementitious mass.
ACI's 2025 SP-366 review dates the change from cement-only to total cementitious mass for these limits to ACI 318-19. Keep the ingredient calculation or hardened-concrete test basis with the result. Chloride ion, salt content and total mass of an admixture are different quantities. A producer's line item naming a chloride-bearing ingredient needs its chloride contribution resolved before the submitted percentage is meaningful.
NRMCA describes two documentation routes: a conservative calculation of total chloride contributed by the ingredients, or ASTM C1218/C1218M water-soluble chloride testing at 28 to 42 days. Identify the route on the submittal so a total-chloride calculation is not mistaken for a different laboratory analyte.
Resolve a class mismatch before ordering the mix
Send the design reviewer a short comparison identifying the member, anticipated service, drawing edition, submitted classes and the requirement that changes. Request a resolved exposure schedule tied to the approved mix number. This is more useful than asking whether a generic exterior mix is acceptable, because the disagreement is visible and traceable.
Keep separate rows for an elevated slab, a buried wall and an interior slab even when the producer offers one mix for all three. Once the classification is resolved, carry the approved identifier into ready-mix ordering.
Distinctions
- Polished-concrete aggregate exposure
- Describes the aggregate revealed by grinding. It is a finish description and does not establish the durability class of the concrete member.
Frequently asked questions
Does publication of ACI 318-25 change an existing project specification?
Publication and project adoption are separate events. Identify the edition incorporated by the governing code and contract, and resolve changes through the design documents before substituting class labels.
Sources checked
Also defined as
- The ACI 318 service condition (F, S, W, C) that sets the maximum w/cm and minimum strength for durability