ANVILFIELD Try FieldOS

Field glossary · material

SCM

SCM, supplementary cementitious material, contributes to concrete binding through pozzolanic reaction, hydraulic reaction or both. On a submittal, 180 lb of slag in 600 lb of binder is 30 percent slag by mass. Count slag already inside a blended cement before adding the separately batched quantity, or the reported SCM share will be understated. Ordering only by a replacement percentage leaves the material identity and percentage denominator unresolved.

Supplementary cementitious material such as fly ash, slag, or silica fume; a mineral addition, not a chemical admixture

Used across 4 Anvilfield field guides, most in Concrete.
Updated

Which specification belongs on the SCM certificate?

As of November 5, 2026, ASTM lists C618-26 for coal ash and raw or calcined natural pozzolans, C989/C989M-26 for slag cement, and C1240-20 for silica fume. Use the material's actual designation and the project-required edition when matching a certificate to a delivery.

ASTM C989/C989M-26 recognizes slag cement strength grades 80, 100 and 120; those grade numbers are not percentages of slag in the concrete. A certificate identifying Grade 120 answers a material-classification question, while the batch sheet supplies the quantity used.

ASTM's C618-26 public scope excludes residues from fluidized-bed combustion and specified refuse-incineration sources. Describing a powder as recycled ash does not establish that it qualifies under C618. Preserve the source and compliance certificate with the approved material identity. The admixtures guide explains where SCMs sit alongside chemical admixtures.

Typical percentages depend on the application

FHWA's 2019 paving-concrete technical brief gives typical SCM rates of 15 to 25 percent for Class F fly ash and 35 to 45 percent for slag cement. These are paving-mixture ranges, not limits for every structural application.

NRMCA CIP 30, revised in 2023, reports slag use from 20 to 80 percent of cementitious mass and metakaolin use from 5 to 15 percent. Its broader ranges reflect different strength, workability and durability objectives. A later strength acceptance age and thermal requirements explain why the mass-concrete guide addresses substantially different binder proportions from ordinary flatwork.

Calculate the percentage using the whole binder

A mixture containing 420 lb of portland cement and 180 lb of slag per cubic yard has 600 lb of cementitious material and 30 percent slag: 180 ÷ 600 × 100. Dividing by portland cement alone would give 42.9 percent, which answers a different question. With 240 lb of mixing water, its w/cm is 240 ÷ 600 = 0.40.

Blended cement needs one more accounting step. If the supplier documents 20 percent slag in 500 lb of blended cement, that delivery already contains 100 lb of slag. Add 100 lb of separately batched slag and the mixture contains 200 lb of slag in 600 lb of binder, or 33.3 percent. Count the internal constituent once, and retain the producer's composition basis. Carry that resolved binder total into the water-cement ratio calculation.

Replacement and addition produce different totals. Replacing 180 lb of an original 600 lb cement charge gives the 30 percent mixture above. Adding 180 lb of slag to an unchanged 600 lb cement charge gives 780 lb of binder and only 23.1 percent slag. Write the final constituent masses before comparing either proposal with a specified percentage.

A material certificate does not qualify the whole mixture

A Grade 120 slag certificate classifies the slag's strength activity in a standardized material test; it does not predict the stripping strength of the proposed 30 percent slag concrete. Keep the mixture qualification tied to the actual aggregate, cement, SCM source and admixture combination. A new source with the same slag grade still needs its identity carried into the approval record.

Distinctions

Separately added limestone filler
NRMCA's March 2026 specification guide excludes separately added inert limestone filler from SCM and cementitious-material totals. Limestone incorporated in a compliant blended cement is accounted for within that cement's mass. Do not increase the w/cm denominator merely because a separate powder appears on the batch sheet.

Frequently asked questions

Does more SCM always mean slower early strength?

No. NRMCA CIP 30 distinguishes silica fume from SCMs commonly associated with slower initial strength gain. Use the qualified mixture's results instead of assigning one strength-development pattern to every SCM.

Can two sources of the same SCM be interchanged under one mix number?

The certificate identifies a material source; the mixture qualification establishes performance with that source and proportion. Carry the actual source into the submittal and delivery record so a source change is visible to the party approving the mixture.

Sources checked

Also defined as

  • Supplementary cementitious material such as fly ash, slag, or silica fume, counted in the cementitious total
  • Supplementary cementitious material, fly ash or slag, used to reduce and slow the heat of hydration

Where this shows up

Next step: Map industrial concrete accounts

Back to the full field glossary