ANVILFIELD Try FieldOS

Field glossary · material

Joint adhesive

Joint adhesive is measured along the cold face of an asphalt paving pass; Crafco lists three to four linear feet per pound for its 34524 product on a two-inch overlay. It forms a hot-applied bond with the adjacent mat. Product number, face height and coating thickness determine the takeoff. A membrane beneath the seam and a sealant poured into an existing crack have different locations and quantities.

A hot-applied polymer-modified asphalt run on the cold joint face to bond the new lane to the old edge

Used across 2 Anvilfield field guides, most in Paving.
Updated

Check the product number and heating window

Crafco's January 2026 data sheet for Pavement Joint Adhesive 34524 specifies a minimum application temperature of 380°F and maximum heating temperature of 400°F. That narrow interval belongs to this product, not every hot-poured material in a paving kettle. Record the product number, lot and measured material temperature together. The linked 2019 installation sheet still prints a 350°F minimum; use the newer data sheet's 380°F minimum when documenting this product's application window.

The same Crafco sheet lists typical coverage of three to four linear feet per pound on a two-inch overlay. For 1,200 feet of that joint, the coverage range corresponds to 300 to 400 pounds. That quantity is adhesive for the face; a takeoff based only on the horizontal paved area misses it.

A coated face has a thickness and a timing requirement

INDOT's 2026 Standard Specifications require a one-eighth-inch joint-adhesive layer on the specified cold face, applied the same day and at least 30 minutes before joint construction. The specified interval is a scheduling requirement distinct from waiting for an emulsion to break. Include the application timestamp in the joint record.

Crafco's installation instructions advise against using its Pavement Joint Adhesive with open-graded pavement because it interferes with drainage. Identify the mix family before substituting a heavy face coating for the treatment on the approved detail. Mark the face coating on the longitudinal-joint detail so the crew can distinguish it from a treatment below the mat.

Why a treated core can read differently

Crafco's installation instructions report that the lower specific gravity of the adhesive can reduce measured joint density by one to two percent. That is a material effect to account for in the specified sampling and acceptance arrangement, not permission to add points to a failing result.

Keep the adhesive location, layer height and core position together when interpreting a joint specimen. A core intersecting a thick adhesive band contains a different material proportion from one entirely inside the mat. Use the paving-joint layout to locate the specimen and report whether it includes the coated face.

Distinctions

VRAM
The membrane is applied beneath the planned joint footprint. Joint adhesive coats the cold face; using one name for both obscures location and quantity.

Frequently asked questions

Can leftover crack sealant replace joint adhesive?

Use the approved joint-adhesive product and its application instructions. A material suitable for a routed service crack has not thereby qualified for a paving construction joint.

Sources checked

Where this shows up

Next step: Build a resurfacing territory

Back to the full field glossary