ASTM C260: air-entraining admixture qualification and dosing

An ASTM C260/C260M-24 declaration qualifies an air-entraining admixture as a material; it does not prescribe a fixed dose for every concrete mixture. Qualification includes effects on setting, strength and length change, with laboratory test data developed under C233/C233M. The producer still establishes the dose and addition sequence for the selected cementitious materials. Product identification, qualification evidence and the actual batch quantity belong together in the submittal.

Current edition: ASTM C260/C260M-24 (2024)
Updated

Official publisher page

Applies to

Admixture manufacturers generate compliance data, specifiers select the required material standard, and concrete producers establish mixture-specific use. The distinction between C260 air entrainers and C494 chemical admixtures in the admixture guide also belongs on the product register, where each submitted formulation needs its own qualification and dosing basis.

Key topics

What does the admixture qualification measure?

ASTM C260/C260M-24 identifies initial and final setting, compressive and flexural strength, and length change among its qualification requirements. The companion C233/C233M-26 develops data for comparison with C260 under standardized laboratory conditions rather than simulating a jobsite. A compliance letter and a project trial batch therefore answer different questions: whether the product qualifies and how the proposed combination behaves.

Read the denominator on the dosage instruction

Euclid's EUCON AEA-92 data sheet, revision 03.21, gives a typical dose of 0.1 to 4 fluid ounces per 100 pounds of total cementitious material for 3% to 6% air. That denominator includes supplementary cementitious material. The published range is a product-specific starting range, not the C260 requirement or an exposure-class target. Preserve the approved dose and its units on the batch instruction.

Separate dispenser setup from stock-condition checks

Euclid directs EUCON AEA-92 to enter the mix separately from other admixtures, preferably onto the sand, and states a 2-year shelf life in its original unopened container. The same sheet calls for protection from freezing; after freezing and thawing it requires thorough agitation and prohibits agitation with air. Record the lot and conditioning history at the dispenser. A product that qualifies under C260 still needs its own storage and handling instructions.

How it is used in the field

At an approved AEA-92 dose of 0.5 fluid ounce per 100 pounds and 600 pounds of total cementitious material per cubic yard, the batch quantity is 3 fluid ounces per cubic yard. A 10-cubic-yard load requires 30 fluid ounces. With 450 pounds of cement and 150 pounds of slag, calculating from cement alone would give only 22.5 fluid ounces for that load, a 25% shortfall from the selected instruction.

Write the batch instruction with the complete material basis, not just “0.5 dose.” Preserve the product formulation, dispenser setting and measured quantity. When a cementitious source or another admixture changes, carry that change into the trial-batch record. The air-entrainment guide covers delivered air behavior; the material qualification should remain traceable through those production changes.

C260 distinguishes samples for quality testing from samples for uniformity testing. ASTM describes a composite admixture sample as combining at least three grab samples. When a supplier provides test evidence for a shipment, retain the sampling description and lot identification with it. A sample of the admixture itself is different from the fresh-concrete sample used to measure delivered air.

Frequently asked questions

Does C260 compliance guarantee the specified air at the forms?

It qualifies the admixture material. The producer’s approved combination and dosing instruction establish its use, and fresh-concrete testing verifies the delivered result. Keep material qualification and placement air records linked by the mix and product identifiers.

Is C233 the same document as C260?

C260 is the material specification. C233 is the testing method used to develop comparison data. As of November 5, 2026, the publisher lists C260/C260M-24 and the newly updated C233/C233M-26.

Does oz/100 lb mean weighing ounces of admixture?

The cited AEA-92 instruction pairs ounces with milliliters, so its dose is a liquid volume per mass of total cementitious material. A dispenser measuring mass needs the product's density to convert that volume. Record fluid ounces explicitly so an operator does not substitute avoirdupois ounces.