ANVILFIELD Try FieldOS

ASTM International

ASTM C42: concrete core strength, conditioning and acceptance

Coring a placement produces a specimen result, not an automatic strength-acceptance decision. Under ASTM International’s C42/C42M-20, extraction, preparation, geometry and conditioning control how that result is obtained. Length and splitting-tension results also fall within the core method; sawed-beam flexure is addressed in appendix recommendations. Identify the core’s location and moisture history with the reported strength, then apply the acceptance criteria selected for the construction investigation or existing-structure evaluation.

Current edition: ASTM C42/C42M-20 (2020)
Updated

Official publisher page

Applies to

Testing laboratories, structural designers and inspection agencies use C42 when an investigation needs physical specimens from hardened concrete. The contractor supplies access and location records; the person reviewing the results needs the sampling plan as well as the compression report. Establish those responsibilities when commissioning the investigation.

Key topics

What does the 85% core acceptance criterion mean?

NRMCA’s March 2026 specification guide states the construction-investigation criteria as a three-core average of at least 0.85f'c and an individual minimum of 0.75f'c. At f'c = 5,000 psi, those checks become 4,250 psi for the average and 3,750 psi for each core. Results of 4,800, 4,500 and 3,700 psi average 4,333 psi: the average passes, but the 3,700 psi specimen fails the individual check. Record both comparisons. This criterion addresses the low-strength construction investigation; it is not a conversion from measured core strength into a design strength for an existing building.

Core orientation belongs in the sampling plan

ASTM C42/C42M-20 identifies both position within the placement and drilling orientation as influences on measured strength: lower concrete tends to be stronger, and loading parallel to the original horizontal placement plane tends to produce lower results. Mark the original top and drilling direction on the location record. Comparing a horizontally drilled wall core with a vertically drilled slab core without those descriptions mixes material differences with specimen orientation. Locate comparison cores in corresponding parts of the placements so elevation and orientation do not become hidden variables.

How long must concrete cores stay sealed?

NRMCA CIP 10 recommends sawing or grinding core ends within two days after drilling and retaining sealed storage for at least five days after the core was last wetted. Those are separate clocks. A core drilled Monday and wet-sawn Wednesday starts the five-day conditioning period on Wednesday. Put extraction, end preparation, last wetting and test times on the laboratory request. ASTM describes this conditioning as a way to make specimens comparable, rather than a reconstruction of the exact moisture distribution inside the member.

Length-to-diameter ratio changes the reported strength

NRMCA CIP 10 recommends a core length-to-diameter ratio near 2 and advises obtaining at least 1.5 where practicable. A 4 in diameter specimen trimmed to 6 in has L/D = 1.5; an 8 in finished length gives L/D = 2. Record finished dimensions, end preparation and any applied correction, rather than just the drill-barrel size. The reviewer needs to distinguish measured failure stress from the final strength reported after specimen corrections.

Separate strength cores from diagnostic samples

ASTM C42/C42M-20 excludes cores from shotcrete and directs that work to C1604/C1604M. A petrographic core, a chloride sample and a compression specimen also have different preparation objectives. Label the intended test before cutting, drying or grinding the sample. The diagnostic-test guide helps allocate material between strength, chemistry and deterioration questions so preparation for one analysis does not consume the evidence needed for another.

How it is used in the field

Build the core register around the actual placement: element, elevation, extraction direction, concrete age, specimen condition and laboratory identifier. Add photographs showing the core before trimming. A damaged end or reinforcement crossing the specimen should appear in the receiving record, where the laboratory and test specifier can decide its disposition before a strength number circulates.

Keep the original core result when comparing it with earlier cylinders. NRMCA CIP 10 states that measured core strengths are not corrected for age. Recasting a later core as an assumed earlier-age cylinder result creates a different calculation and loses the measured evidence. Attach the laboratory report and the reviewer’s interpretation as separate records, then carry the decision into the structural QA turnover.

Frequently asked questions

Does a core need to be tested immediately after drilling?

The preparation and moisture-conditioning schedule determines the test date. Arrange laboratory receiving and sealed storage before drilling so transport delays do not produce undocumented drying.

Can I divide a core result by 0.85 to estimate cylinder strength?

The 0.85 acceptance fraction is not a specimen-strength conversion factor. ASTM C42/C42M-20 describes several influences on the core-to-cylinder relationship, including moisture, consolidation and coring damage. NRMCA CIP 10 distinguishes construction acceptance from the equivalent-strength evaluation used for an existing structure; keep the measured result and the selected evaluation method identifiable.