ANVILFIELD Try FieldOS

Field glossary · measurement

Cessation temperature

Cessation temperature is the internal asphalt-mat cutoff used to end density-building rolling, typically 175 to 180°F (80 to 82°C) in the 2025 Asphalt Paving Handbook. Attach the sensing location to that number: a 168°F infrared surface reading and a 185°F internal probe reading describe different parts of one lift. Compare the specified internal limit with the probe result when deciding whether useful compaction time remains.

The mat temperature below which rolling no longer adds density, the bottom of the compaction window

Used across 2 Anvilfield field guides, most in Paving.
Updated

Which temperature belongs beside the density reading?

ASTM D8673/D8673M-26 says surface and internal asphalt temperatures must not be compared for acceptance because their cooling rates can differ. That distinction matters when a roller-mounted infrared sensor reports surface temperature while a technician records a probe reading within the lift. Label the measurement type before comparing either reading with the specified stopping criterion.

Pair each density observation with a temperature at that location and a known roller-pass count. Keep probe depth and instrument identity fixed through the comparison; otherwise the resulting trend mixes changes in measurement with changes in the mat. The compaction-window guide provides the production plan, while these paired observations locate its density-building endpoint.

An infrared reading after the roller passes

The 2025 Asphalt Paving Handbook, Section 11.7.1.2, recommends a penetration thermometer after a roller has crossed the measurement location because drum spray can cool the surface and distort an infrared reading. A cold infrared patch immediately behind a wet drum therefore needs a different interpretation from a cold patch in untouched mix behind the screed.

Compare readings taken under consistent conditions when developing the rolling pattern. Moving the infrared measurement from dry, unrolled mix to a freshly wetted roller track changes the measurement conditions as well as the elapsed time. Logging that change prevents an apparent temperature drop from becoming a false estimate of the mixture's cooling rate.

Set the cooling model to the tested stopping point

MnDOT's PaveCool documentation allows user-selected starting and stopping compaction temperatures in version 2.4 and later. Its familiar 175°F cooling endpoint is a model input that can be replaced with the project's established limit. Save that setting with the lift thickness and weather inputs so another technician can reproduce the prediction.

With a 180°F project stopping point and a model left at 175°F, the prediction includes cooling through an extra 5°F beyond the planned density-building interval. Change the endpoint before scheduling roller coverage. The resulting time difference comes from the cooling calculation; it cannot be obtained by assuming a constant number of minutes per degree.

Distinctions

Minimum finish-rolling temperature
List the specified finishing temperature beside the finish-rolling operation in the field record. Its purpose is to control mark removal; keep the internal density-building limit in a separate column so the last appearance pass does not become the assumed compaction cutoff.
Tender zone
A temporary loss of stability can interrupt rolling before cessation. Use the observed instability band and the stopping point as separate boundaries when allocating the available time.

Field example

A project uses an internal stopping point of 180°F. At the same station, the surface reads 168°F and the probe reads 185°F. The internal reading is still 5°F above the stopping point; the surface reading is 12°F below that number but does not satisfy the internal measurement criterion. Recheck with the same probe depth as the mat cools, and retain the density result alongside it.

Frequently asked questions

Does a density plateau prove the mix has reached cessation?

No. A plateau also occurs when additional passes with the selected roller setup stop producing gains while the mixture is still hot. Locate cessation from paired temperature and density observations, rather than assigning the last temperature measured to every future lift.

Does a PaveCool result prove that density was achieved?

It predicts cooling time. The corresponding density measurements establish whether the roller train used that interval successfully.

Sources checked

Also defined as

  • The mat temperature below which rolling no longer reduces air voids

Where this shows up

Next step: Build a fall paving list