ANVILFIELD Try FieldOS

Field glossary · component

Galvanic anode

A galvanic anode is a consumable source of corrosion-protection current that operates without a rectifier. For embedded concrete-repair units, acceptance includes two paths: the wire-to-steel connection and conductive mortar between the anode and existing concrete. Vector's Galvashield XP instructions set a 1-ohm maximum DC continuity resistance; satisfying that connection limit still leaves mortar conductivity and complete encapsulation to verify.

A sacrificial zinc element tied to the steel that corrodes preferentially and feeds it a small protective current

Used across 2 Anvilfield field guides, most in Concrete.
Updated

Verify two different electrical paths

Vector's January 2024 Galvashield XP installation instructions accept a maximum DC resistance of 1 ohm, or a potential difference no greater than 1 mV, when verifying electrical continuity. Test the anode connection and continuity of the reinforcing steel served by the repair; a disconnected bar is not protected merely because another bar has an anode.

The second path runs through the repair material to the existing concrete. An insulating bond coat, a void around the unit, or an unsuitable repair mortar can interrupt that path even when the steel-side continuity measurement passes. Separate those checks in the placement record so neither is mistaken for the other.

Repair-mortar resistivity changes the installation

Vector's October 2026 Galvashield XP data sheet requires a conductive mortar path when the repair material has saturated bulk resistivity of 50,000 ohm-cm or greater. For that path it specifies Galvashield Embedding Mortar or another repair mortar with resistivity of 15,000 ohm-cm or less between the anode and substrate.

These are Galvashield XP product criteria, not a spacing rule for every zinc anode. Specify the selected unit and compatible mortar together. The surrounding repair material carries ions, so selecting it solely by compressive strength overlooks an essential part of the corrosion-control system.

Vector's installation instructions call for clear space between anode and substrate of at least 3/4 inch, or 1/4 inch more than the largest repair aggregate, whichever is greater. With 3/4-inch aggregate, the resulting minimum is 1 inch. Measure the actual gap around the installed unit, because its mortar shell and tie-wire position consume space within the repair cavity.

Use the inspection readings to find the interruption

One anode connection measures 0.4 ohm and another measures 2.3 ohms. The second exceeds the cited 1-ohm continuity limit and needs its connection corrected before concealment. Passing that retest still leaves the mortar conductivity and encapsulation checks to complete.

A repair record for perimeter anodes should identify the model, installed positions, continuity readings, repair mortar, and any separate embedding mortar. An anode count cannot explain a failed circuit when the connection or the ionic path is missing.

Distinctions

Impressed-current anode
An impressed-current system uses an external power source. A galvanic unit is driven by the potential difference between its metal and the steel.
Barrier coating
A barrier blocks exposure or current paths. A galvanic anode requires an intentional conductive circuit to perform its function.

Frequently asked questions

Can epoxy isolate an otherwise well-tied anode?

Yes. Vector warns against insulating epoxy bonding agents and against coating the anode or its wire connection. Electrical attachment and ionic contact must both remain effective.

Is the largest anode always the right choice?

Selection includes current demand, connected steel area, exposure, and the specified distribution. More zinc at one location does not establish current distribution throughout the repair.

Sources checked

Where this shows up

Related guides

Next step: Locate rehabilitation contracts

Back to the full field glossary