Field glossary · property
CSP
CSP, concrete surface profile, is assigned by matching prepared concrete to ICRI texture comparators: a CSP 4 record identifies a class rather than a 4-mil depth. Specify the required comparator and the areas it applies to. Where profile depth also matters, measure and report it separately, retaining a labeled replica when later review of the concealed texture is needed.
Concrete surface profile, the ICRI roughness scale for a prepared bonding surface, higher numbers rougher
Why CSP numbers do not convert directly to mils
ICRI Guideline 310.2R-2013 includes CSP 10, the additional aggressive profile introduced for concrete repair. Older references that stop at CSP 9 omit that profile. The comparators represent different prepared textures; they are not ten equal steps on a depth ruler.
A CSP 4 requirement therefore does not mean a 4-mil surface or a texture twice as deep as CSP 2. Record the comparator result as a CSP class. Where a specification also requires a measured depth, record that result separately with its instrument and units. Peaks, valleys, and the spacing of features all affect how a texture compares.
Keep a profile record after the coating hides it
ASTM D7682-17(2022) describes making a permanent concrete-surface replica with putty for comparison with visual standards or measurement of profile depth. A labeled replica preserves more evidence than a photograph taken under an unknown light angle.
Index each replica to a floor plan or repair location and identify the prepared area it represents. A single favorable patch at the equipment setup point does not document a doorway, wall edge, or hand-ground penetration surround. Those areas often receive different preparation equipment and deserve separate records.
ASTM D8271-26 is the current method for measuring profile depth directly on prepared concrete. Its depth result and a D7682 replica answer different documentation needs: the direct reading quantifies the surface, while the retained replica lets another inspector revisit its texture after coating. Specify the method alongside the required CSP class.
Resolve a roughness dispute before primer
A floor specification calls for CSP 4. The main shot-blasted field compares with that reference, but a hand-ground perimeter compares with CSP 2. Treat the perimeter as a separate preparation area and correct its texture before accepting the whole floor. Averaging the two CSP numbers would invent a measurement the comparator system does not provide.
Preserve the profile record at the resinous-flooring handoff and after preparing a concrete repair cavity. Pair it with separate cleanliness and moisture results so later adhesion failures can be compared with the substrate actually accepted.
Distinctions
- Surface cleanliness
- A retained profile replica documents the concrete's geometry. It supplies no acceptance result for oil contamination or residual dust, which need their own inspection evidence.
- Dry film thickness
- Dry film thickness measures the cured coating. Surface-profile depth measures the concrete beneath it.
Frequently asked questions
Is CSP 10 a real ICRI profile?
Yes. ICRI added it in the 2013 guideline revision for more aggressive concrete repair preparation.
Can I specify CSP using only a micrometer number?
Specify the required texture class explicitly when the system calls for CSP. A numerical depth supplements that requirement; it is not an automatic conversion to a comparator class.
Sources checked
Also defined as
- Concrete surface profile, the ICRI roughness scale from CSP 1 (smooth) to CSP 9 to 10 (coarse)
- Concrete surface profile, the ICRI 1 to 10 roughness scale that grades the prepared slab