ANVILFIELD Try FieldOS

Field glossary · material

Trackless tack

Trackless tack is an asphalt bonding emulsion formulated to resist tire pickup, with readiness determined for the supplied product. SpecChem's MAX-A-TACK TTC sheet specifies a minimum 10-minute break time; that is a break criterion, not a guaranteed traffic-release time. FHWA defines set as complete water evaporation, a separate stage from the brown-to-black break. Record the product, film condition, and residual binder rate before releasing the treated area to the next operation.

An engineered emulsion that breaks to a hard, non-sticky film so traffic and equipment do not pick it up

Used across 2 Anvilfield field guides, most in Paving.
Updated

Read the product approval beyond its trackless label

FHWA-HIF-16-017 describes reduced-tracking formulations that use stiffer base binders, chemical modifications, or both. The commercial label describes the handling result; the supplied grade and project approval identify the material. Put the approved product, shipment identification, residue basis, and supplier's spray and storage instructions on the distributor record.

Tire pickup and interface bonding are different observations. A film that survives haul traffic answers the handling question. The overlay still needs the specified binder quantity and a bond to the receiving surface. Carry those acceptance records into the mill-and-overlay work rather than closing the tack inspection after a pickup observation.

Brown-to-black break and water-free set are separate stages

FHWA's 2016 Tack Coat Best Practices separates the brown-to-black break from the later water-free set, so a field log needs distinct observations when the paving release calls for set. Writing black at 10:20 records a color change; it does not record complete drying at 10:20. Keep the required release condition explicit on the distributor and paving records.

The online Asphalt Paving Handbook, section 5.5.3, identifies emulsion grade, application rate, surface temperature, and environmental conditions as controls on evaporation. More applied water requires more drying. A coat remaining wet in shaded milling grooves needs its own observation even when the exposed ridges have changed color. Keep the observed stage and location with the paving release.

Read a manufacturer's applied rate and break time together

SpecChem's MAX-A-TACK TTC technical sheet, revised February 19, 2018, specifies distributor application at 0.05 to 0.10 gal/sq yd and 130°F to 160°F, with a minimum break time of 10 minutes. Those are this product's applied-emulsion rates and distributor temperatures. They are not residual-binder rates, pavement-temperature minima, or a promise that the film has set in ten minutes.

The same sheet lists a 50% minimum residue by distillation. That lower limit shows why FHWA's general 57% to 70% range cannot replace the shipment's actual residue value in a distributor calculation. Use the approved supplier's residue and mass-to-volume basis for the material on the truck.

Convert residual gallons to the distributor setting

FHWA-HIF-16-017 gives typical undiluted-emulsion residual asphalt contents of 57% to 70%. Its application-rate table uses a 67% asphalt assumption. The product's actual residue and the specified conversion basis belong in the calculation, particularly when a certificate expresses residue by mass and the distributor reports volume.

Using FHWA's 67% volumetric calculation assumption, 2,000 sq yd at 0.06 gal/sq yd residual requires 120 gallons of binder and about 179 gallons of undiluted emulsion: 120 / 0.67. The corresponding distributor rate is about 0.090 gal/sq yd. Calling 0.06 the spray rate would leave only about 0.040 gal/sq yd under that assumption.

The residual-rate entry carries the quantity distinction. Trackless designation does not authorize dilution. Use the approved product's instructions and the project's dilution permission when establishing the supplied emulsion rate.

Compare meter totals at the same temperature basis

The Asphalt Paving Handbook reports asphalt-emulsion volumes at 60°F and applies temperature corrections when verifying distributor quantities. A hot tank volume and a temperature-corrected delivery volume need that common basis before they establish consumption over the sprayed area.

Record spray width, travel distance, corrected emulsion usage, and the residue calculation together. A matching whole-job gallon total still leaves local skips unresolved, so retain the coverage inspection alongside the arithmetic. The tack and prime guide explains surface preparation and the surrounding spray operation.

Frequently asked questions

Does trackless mean the coat is ready after ten minutes?

SpecChem labels ten minutes as a minimum break time for MAX-A-TACK TTC, not a set-time or traffic-release guarantee. The release record needs the stage required by the approved product instructions and the observed condition in the slowest-drying part of the shot.

Are tanker gallons the same as residual gallons?

Under FHWA's 67% volume assumption, 100 gallons of emulsion represents 67 gallons of residual binder after water removal. Both volumes must use the same reference temperature. The delivered product's actual residue basis replaces that assumption when reconciling a shipment.

Sources checked

Also defined as

  • A proprietary tack that sets fast and does not pick up on truck tires, so coverage survives to the paver

Where this shows up

Next step: List industrial yard accounts